Lapox Powergrip is two component modified, viscous epoxy adhesive system. When both components are mixed in recommended ratios and cured appropriately at room temperature, an excellent bond strength can be achieved with most of the substrates including glass, metals, reactive plastics, wood, textile and natural stones. Faster productivity can be achieved, if curing is performed at higher temperature between 40°C and 60°C. Curing at higher temperature is recommended to achieve optimum bond strength.
Test | Unit | Reference | Resin | Hardener |
---|---|---|---|---|
Description | --- | Visual | Clear viscous liquid | Clear, yellowish to brownish, viscous liquid |
Viscosity at 25°C1 | m Pas | ASTM D2196 | 35,000 - 45,000 | 28,000 - 40,000 |
Colour | GS | ASTM D1544 | --- | Max 8 |
Colour | APHA | ASTM D1209 | Max 100 | --- |
Density | g/cc | ASTM D792 | 1.04 - 1.12 | 0.92 - 0.98 |